Polyamide 66 dyed mono yarn
Material: 100% Polyamide 66
Yarn Section: round, trilobal as per customer's request
Specification: 10D/1F, 12D/1F, 15D/1F, 20D/1F, 30D/1F, 40D/1F, 53D/1F (0.08mm), 0.10mm, 0.12mm, 0.15mm, 0.16mm, 0.18mm, 0.20mm, 0.23mm, 0.25mm to 5.0mm
Packing: wrapped on steel cops, paper cops, plastic bobbins
Color: raw white, dope dyed with varied colors according to customers requirement.
Advantage and Characteristics of yarn: excellent eveness of diameter, high tenacity, low shrinakge, this makes our yarns perform well in the techinical fabric area.
End use: warping and wefting yarn in common textile, sewing thread and ribbons, filtration fabric, screen printing fabric, fishing lines, tyre cord fabric and related industrial textiles.
Material: 100% Polyamide 66
Yarn Section: round, trilobal as per customer's request
Specification: 10D/1F, 12D/1F, 15D/1F, 20D/1F, 30D/1F, 40D/1F, 53D/1F (0.08mm), 0.10mm, 0.12mm, 0.15mm, 0.16mm, 0.18mm, 0.20mm, 0.23mm, 0.25mm to 5.0mm
Packing: wrapped on steel cops, paper cops, plastic bobbins
Color: raw white, dope dyed with varied colors according to customers requirement.
Advantage and Characteristics of yarn: excellent eveness of diameter, high tenacity, low shrinakge, this makes our yarns perform well in the techinical fabric area.
End use: warping and wefting yarn in common textile, sewing thread and ribbons, filtration fabric, screen printing fabric, fishing lines, tyre cord fabric and related industrial textiles.
Model |
Diameter
(mm) |
Diameter
Deviation
(mm) |
Breaking
Strength
(N)≥ |
Tenacity
(CN/Tex),≥ |
Elongation
At break
(%) |
Free shrinkage in hot air @ 180ºC×10min(%) |
VS20A |
0.18 |
±0.01 |
14.5 |
50 |
34 |
4.5±1 |
|
0.20 |
±0.01 |
18 |
50 |
34 |
4.5±1 |
|
0.23 |
±0.01 |
23.5 |
50 |
32 |
4.5±1 |
|
0.27 |
±0.015 |
33.3 |
51 |
32 |
4.5±1 |
|
0.30 |
±0.015 |
41 |
51 |
32 |
4.5±1 |
VS20B |
0.15 |
±0.008 |
14.3 |
70 |
17 |
8.5±1 |
|
0.17 |
±0.01 |
19 |
72 |
17 |
8.5±1 |
|
0.20 |
±0.01 |
24 |
66 |
17 |
8.5±1 |
|
0.22 |
±0.01 |
28 |
66 |
17 |
8.5±1 |